A bead blaster would give you that satin finish in no time flat...
Regards,
Jeff
> About the only common material that sodium
hydroxide will attack is
> aluminium, and then only when concentrated or exposure is reasonably long;
> it has no effect on copper, steel, etc.
Yeah, I've relied on this as a way to make
satin-finish aluminum front
panels for equipment. As the reaction progresses, the NAO2 (?) solution
has to be preiodlically replaced. It generally took me about two days to
get the desired look.
-dq
--
-----------------------------------------------------------
Jeffrey S. Worley
Asheville, NC USA
828-6984887
UberTechnoid(a)Home.com
-----------------------------------------------------------