On Aug 1, 2015, at 8:28 PM, Chuck Guzis <cclist at
sydex.com> wrote:
...
I never use RoHS solder--it simply doesn't wet or flow like 67/37 Sn/Pb solder. The
exception is SMT where components are mounted using solder paste (powered solder+flux).
If I could find some of the leaded stuff, I'd probably use it.
It?s still around. Check for example
www.stanleysupplyservices.com, look for solder,
Kester, keyword ?paste?. The first item that came up in my search is 63/37 real solder
paste. There are a bunch of entries, packages of different sizes and different flux
types.
paul