On Thu, Jul 17, 2008 at 7:26 AM, Mike Loewen
<mloewen at cpumagic.scol.pa.us> wrote:
I have a HP 2647A terminal with a severe case of screen rot which I would
like to refurbish:
http://sturgeon.css.psu.edu/~mloewen/Oldtech/Terminals/HP2647A-1L.jpg
http://sturgeon.css.psu.edu/~mloewen/Oldtech/Terminals/
Do you think this would be a candidate for the heat gun method, or acetone
around the edges of the shield as others have suggested?
There is also the nichrome wire method which has been used on HP 264x
terminal CRTs:
http://www.classiccmp.org/pipermail/cctalk/2005-February/059554.html